ASTM B963 – Standard Test Methods for Oil Content, Oil-Impregnation Efficiency, and Surface-Connected Porosity of Sintered Powder Metallurgy (PM) Products Using Archimedes’ Principle
Description:
Significance and Use
5.1 Oil content values are generally contained in specifications for oil-impregnated PM bearings.
5.2 The oil-impregnation efficiency provides an indication of how well the as-received parts had been impregnated.
5.3 The desired self-lubricating performance of PM bearings requires a minimum amount of surface-connected porosity and satisfactory oil impregnation of the surface-connected porosity. A minimum oil content is specified.
5.4 The results from these test methods may be used for quality control or compliance purposes.
Scope
1.1 This standard describes three related test methods that cover the measurement of physical properties of oil-impregnated powder metallurgy products.
1.1.1 Determination of the volume percent of oil contained in the material.
1.1.2 Determination of the efficiency of the oil-impregnation process.
1.1.3 Determination of the percent surface-connected porosity by oil impregnation.
1.2 Units—With the exception of the values for density and the mass used to determine density, for which the use of the gram per cubic centimetre (g/cm3) and gram (g) units is the long-standing industry practice, the values in SI units are to be regarded as standard. The values given in parentheses after SI units are provided for information only and are not considered standard.