• Skip to main content
  • Skip to header right navigation
  • Skip to site footer
MAT-CS - Materials Characterization Services

Materials Characterization Services

  • Home
  • About
    • Meet the Team
    • Consulting
  • Analytical Techniques
    • Bulk Analysis
    • Microscopy and Microanalytical
    • Surface and Thin Film
    • Polymer Characterization
    • Optical Measurements
    • Liquids and Gases
    • Electrical / Electronics
    • Reliability Testing
    • Miscellaneous
  • Test Methods
    • ASTM Methods List
    • ISO Methods List
    • AATCC
    • AOAC
    • AOCS
    • EPA, SM
    • FDA BAM
    • IP
    • JEDEC
    • MIL-STD
    • OCSPP
    • OPPTS
    • REACH
    • RoHS
    • SEMI
    • TAPPI
    • USP/EP/JP
  • Resources
    • Experiment Design
    • Consulting
    • The Laboratory Landscape
    • Quality Programs
    • Regulatory-Based Analyses
  • Contact Us
  • Get a Quote!
MAT-CS Home Cover

ASTM D465

ASTM D465 – Standard Test Methods for Acid Number of Pine Chemical Products Including Tall Oil and Other Related Products

Description:

Significance and Use

3.1 These test methods are designed to broaden the scope of the earlier editions of the test method by the inclusion of tall oil and tall oil derived products as test materials and will be referenced in Test Methods D803.

3.2 The acid number is an important property of pine chemical products, such as tall oil, and the products obtained by the fractionation of tall oil. It is the test method widely used to determine the total free acid content of these products.

3.3 The potentiometric test method should be used when the most reproducible results are required.

Scope

1.1 These test methods are intended for determining the acid number of pine chemical products as defined in Terminology D804 including tall oil products, wood and gum rosin, and other related materials. These test methods may not be applicable to all modified rosin products. Two test methods are covered, as follows:

1.1.1 Potentiometric method (referee), and

1.1.2 Internal indicator method (alternate).

1.2 The potentiometric method is suitable for use with both light- and dark-colored products. It should be considered the referee method. The internal indicator method is suitable for use only with light- and medium-colored products with a Gardner color of less than 12. It should be considered the alternate method.

1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

Related Test Methods

ASTM D5208

ASTM D5206

ASTM D5201

ASTM D5200

ASTM D5199

ASTM D5198

ASTM D5194

ASTM D5191

ASTM D5190

ASTM D5188

ASTM D5187

ASTM D5186

Previous Post:MAT-CS Home CoverASTM D4648
Next Post:ASTM D4658MAT-CS Home Cover

Ready to start your analysis?

Get a Quote!
MAT-CS

Your One Source for Materials Analysis

1-800-685-2088

support@mat-cs.com

  • Home
  • Analytical Techniques
  • Test Methods
  • Resources
  • Contact Us
  • Get a Quote!
  • Special Analysis Request

  • LinkedIn

Copyright © 2026 Materials Characterization Services · A Covalent Corp. · All Rights Reserved